Title: Biaxial Inelastic Frame Seismic Behavior

Author(s): Lawerence G. Selna and John H. Lawder

Publication: Symposium Paper

Volume: 53

Issue:

Appears on pages(s): 439-462

Keywords: biaxial loads; ductility; dynamic stuctural analysis; earthquake resistant structures; earthquakes; frames; lateral pressure; loads (forces); mathematical model; moment-curvature relationship; reinforced concrete; static structural analysis

DOI: 10.14359/17706

Date: 1/1/1977

Abstract:
The importance of overturning forces and biaxial repsonse is studied for 3D reinforced concrete frame structures subjected to biaxial inputs. A biaxial yield rule is used for the moment-curvature relation.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer