Title: Time-Dependent Properties of Concrete Containing a Superplasticizing Admixture

Author(s): J.J. Brooks, P.J. Wainwright, and A.M. Neville

Publication: Symposium Paper

Volume: 62

Issue:

Appears on pages(s): 293-314

Keywords: admixtures; compressive strength; concrete durability; concretes; creep properties; creep recovery; dynamic modulus of elasticity; mechanical properties; modulus of elasticity; plasticizers; shrinkage; tests; ultrasonic tests; workability

DOI: 10.14359/17730

Date: 1/1/1979

Abstract:
Strength, elasticity, durability, creep and shrinkage of concretes with and without a superplasticising admixture have been compared over a period of one year.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer