Shear Transfer in Concrete Having Reinforcement at an Angle to the Shear Plane

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Transfer in Concrete Having Reinforcement at an Angle to the Shear Plane

Author(s): A.H. Mattock

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 17-42

Keywords: cracking (fracturing); loads (forces); precast concrete; reinforced concrete; reinforcing steels; research; shear properties; stress transfer; structural analysis; tests

DOI: 10.14359/18149

Date: 1/1/1974

Abstract:
This paper presents and experimental and analytical study of shear transfer across a plane inclined at an arbitrary angle to a parallel or orthogonal array of reinforcement.




  