Experimental Study of Recovered Properties of Retrofit (Repaired) Concrete Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study of Recovered Properties of Retrofit (Repaired) Concrete Members

Author(s): K. Suzuki and A. Fujii

Publication: Symposium Paper

Volume: 237

Issue:

Appears on pages(s): 27-36

Keywords: confined concrete; reinforced concrete; repair; retrofit; seismic performance

DOI: 10.14359/18240

Date: 8/1/2006

Abstract:
Two interior column (RC)-beam (PPC) specimens were tested. The specimens were first subjected to reversed, repeated cyclic loading to maximum rotational angles of 1/30 and 1/16, respectively. The specimens were then repaired using resin injection and mortar covering. Mechanical properties obtained following repair were almost the same as those obtained during the initial loading, probably, due to the confined concrete used in the beam ends. However, a reduction in initial stiffness of approximately 30% was observed.




  