Title: Revised Standard for Plywood and Overlays

Author(s): Steve Zylkowski and Dave Gibson

Publication: Concrete International

Volume: 29

Issue: 6

Appears on pages(s): 26-29

Keywords: formwork; overlay; plywood; standard

DOI:

Date: 6/1/2007

Abstract:
US Voluntary Product Standard PS 1 establishes minimum requirements for plywood and provides manufacturing specifications such as species, veneer thicknesses, grades, and performance requirements for certain end uses. This article highlights the changes in the recently published PS 1-07 standard, “Structural Plywood,” that pertain to overlaid plywood panels for concrete formwork. With the new standard, end users will be able to more accurately specify concrete forming panels according to their primary application and desired performance.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.