Evaluating Drying Shrinkage of Self-Compacting Concrete in a Caisson Using Numerical Methods

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluating Drying Shrinkage of Self-Compacting Concrete in a Caisson Using Numerical Methods

Author(s): T.H. Liu, H.J. Chen, H.W. Liao, and C.I. Lin

Publication: Symposium Paper

Volume: 243

Issue:

Appears on pages(s): 85-98

Keywords: caisson foundation; drying shrinkage; self-compacting concrete

DOI: 10.14359/18745

Date: 4/1/2007

Abstract:
Self-compacting concrete (SCC), characterized by the high flowability and high re-sistance to segregation, is due to the high amount of paste (including cement and mineral admixtures) in contrast with normal concrete (NC). However, the high amount of paste will limit the volume fractions of coarse aggregate and reduce the tendency of coarse aggregate to suppress drying shrinkage deformations. For this reason, SCC can be expected to produce higher values of drying shrinkage than NC. In order to assess the drying shrinkage of SCC quantitatively for application to offshore caisson foundations, the formulas presented in the literature (ACI 209 and CEB-FIP) are used to predict the values of drying shrinkage in SCC according to the cor-responding mixture proportioning. Additionally, a finite element (FE) model, which as-sumes concrete to be a homogeneous and isotropic material and follows the actual size and environmental conditions of the caisson, is utilized to simulate situations of stress distribution and deformations in the SCC caisson resulting from the drying shrinkage. The likelihood of cracking and the behavior of drying shrinkage of the SCC caisson are drawn from the analytic results calculated by the FE model proposed in this paper.




  