International Concrete Abstracts Portal

  


Title: Delivering Practical Solutions to the Concrete Industry

Author(s): Joseph Sanders and Claude Bedard

Publication: Concrete International

Volume: 30

Issue: 7

Appears on pages(s): 27-28

Keywords: ACI Foundation; Charles Pankow Foundation; funding; research

DOI:

Date: 7/1/2008

Abstract:
To help innovative research make the final leap from the lab to the field, the ACI Foundation and the Charles Pankow Foundation signed a 3-year agreement at the ACI Spring 2008 Convention in Los Angeles, CA. The ACI Foundation will help identify industry research needs and recommend worthy projects. The Charles Pankow Foundation will then select, fund, and manage research projects that meet its criteria. The ACI Foundation will also help disseminate the research results to reach a wide range of industry users.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.