Title: Concrete Q & A: What Is Mass Concrete?
Author(s):
Publication: Concrete International
Volume: 25
Issue: 12
Appears on pages(s): 112
Keywords:
DOI:
Date: 12/1/2003
Abstract: When is a structural section large enough to be defined as mass concrete? We’re concerned about the potential for thermal cracking caused by heat of hydration in a structure that isn’t a dam but is of fairly massive size.