Title: Subsequently Applied Waterproof Basements Made of Textile Reinforced Concrete Using the Spraying Method

Author(s): R. Mott and W. Brameshuber

Publication: Symposium Paper

Volume: 251

Issue:

Appears on pages(s): 59-72

Keywords: fabrics; fine-grained concrete; material properties; production technology; spraying technique; subsequent sealing; textile-reinforced concrete; waterproof construction

DOI: 10.14359/20150

Date: 3/1/2008

Abstract:
Many regions in Germany show a rising groundwater level. Hence, the load case of buildings concerned changes from non-pressing to pressing water. Residential buildings not designed for the load case of pressing water have to be refitted. Conventional sealing methods are often associated with high complexity and high costs as well as the loss of living space. Furthermore, in many cases, they do not consider the additional static load of pressing water at all. This paper presents a newly developed, subsequently applied sealing against pressing water. It is made of textile-reinforced concrete. Using this composite material, it is possible to produce a sealing system with a wall thickness of about 30 to 35 mm (1.18 to 1.38 in.). During the production of an exhibit wall, it became apparent that the spraying technique is an adequate and practicable method to produce a subsequent sealing of textile reinforced concrete. Initial observations of the wall subjected to hydrostatic pressure reveal the application potential of this construction.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer