Title: Permeability of Selected Concretes

Author(s): D. Whiting

Publication: Symposium Paper

Volume: 108

Issue:

Appears on pages(s): 195-222

Keywords: absorption; chlorides; concretes; moist curing; permeability; porosity; silica fume; tests; voids; water-cement ratio; Materials Research

DOI: 10.14359/2186

Date: 8/1/1988

Abstract:
Study of permeability was made using six concrete mixtures ranging in water-to-cementitious material (w-c) ratio from 0.26 to 0.75. Concrete specimens were tested for permeability to water and air, permeability to chloride ions (rapid and long-term), volume of permeable voids, and porosity. Results confirm that permeability is a direct function of w-c ratio. The addition of silica fume results in even greater decreases in permeability than would be anticipated based solely on w-c ratio. A period of initial moist curing of at least seven days is essential for achieving low permeability. Results also indicate that rapid test procedures offer a reasonable alternative to more lengthy and complex conventional permeability tests.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer