Title: Properties of No-Fines Concrete Containing Silica Fume

Author(s): Motoharu Tamai

Publication: Symposium Paper

Volume: 114

Issue:

Appears on pages(s): 799-814

Keywords: coarse aggregates; compressive strength; flexural strength; freeze-thaw durability; modulus of elasticity; no-fines concrete; permeability; plasticizers; silica fume; thickness; Materials Research

DOI: 10.14359/2395

Date: 5/1/1989

Abstract:
Cement paste with silica fume was used to improve strength and other characteristics of no-fines concrete. The results showed that by using cement paste with silica fume and superplasticizer, apparent viscosity and yield value of the paste in the fresh stage can be controlled. The compressive strength of no-fines concretes with silica fume is in the range of 20 to 47 MPa. Other characteristics such as flexural and splitting strengths, modulus of elasticity, and frost resistance of no-fines concrete are improved. The coefficient of water permeability varies depending on the amount of the continuous void and binder. A value of 2 to 50 mm/sec can be obtained.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.