Title: Computer Evaluation of the Effect of Prestressing on a Shell Structure

Author(s): Jeanne M. Nagele, Sankar C. Das, and Reda M. Bakeer

Publication: Symposium Paper

Volume: 120

Issue:

Appears on pages(s): 409-424

Keywords: computer programs; domes (structural forms); evaluation; jacking; nuclear reactor containment; prestressed concrete; prestressing; prestressing steels; shells (structural forms); structural analysis; Structural Research

DOI: 10.14359/2862

Date: 6/1/1990

Abstract:
The purpose of this investigation was to examine the forces developing in the dome of a prestressed concrete nuclear containment structure due to prestressing of vertical tendons. A computer program was developed for personal computers to evaluate the effect of prestressing forces. A parametric study was conducted, using the program, to examine the effects of dimensions, prestressing force, properties of tendons, etc. on the resulting stresses in the dome.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer