Title: Concrete Supplier Fills Tall Order

Author(s): Michael F. Pistilli, Al Cygan, and Leonard Burkhart

Publication: Concrete International

Volume: 14

Issue: 10

Appears on pages(s): 44-47

Keywords: admixtures; conveying; high-rise buildings; pumped concrete; high-strength concrete; quality control; ready-mixed concrete; Construction

DOI:

Date: 10/1/1992

Abstract:
Describes construction of the world's tallest reinforced concrete building from the ready-mix supplier's perspective, with regard to materials, jobsite quality control, the concrete's statistical performance, project coordination, and using state-of-the-art technology. The good communication and teamwork that led to the successful completion of the project should serve as a helpful model for future jobs of this size and stature.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.