Title: Laboratory Experience With the Rapid Chloride Permeability test

Author(s): B. Mobasher and T. M. Mitchell

Publication: Symposium Paper

Volume: 108

Issue:

Appears on pages(s): 117-144

Keywords: aggregate gradation; air entrainment; chlorides; concretes; coarse aggregates; permeability; tests; water-cement ratio; General

DOI: 10.14359/3621

Date: 8/1/1988

Abstract:
The new rapid chloride permeability test, in which chloride ions are driven into concrete samples electrically over a 6-hr period, is becoming widely used and has been accepted as an American Association of State and Highway Transportation Officials (AASHTO) standard, T277. This paper summarizes the results of an extensive series of laboratory tests with the new method. Results of an interlaboratory test program provide single-operator and multilaboratory coefficients of variation suitable for use in a precision statement in the standard versions of the method. Several possible revisions to the AASHTO standard procedure are examined, but further study is necessary before any can be accepted. Test results on specimens with diameters other than the standard 3.75 in. (95 mm) called for in T277 are found to be easily adjusted to allow comparisons with standard size specimens. Several fundamental properties of concrete, namely, water-cement ratio, coarse aggregate type and gradation, and air content, are shown to affect chloride permeability.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer