International Concrete Abstracts Portal

  


Title: Laboratory Permeability Measurement

Author(s): D. J. Janssen

Publication: Symposium Paper

Volume: 108

Issue:

Appears on pages(s): 145-158

Keywords: concretes; measuring instruments; permeability; samples; tests; test equipment; General

DOI: 10.14359/3633

Date: 8/1/1988

Abstract:
Equipment and procedures for measuring actual permeability of portland cement concrete are presented. The equipment is built from readily available parts and materials and requires only standard laboratory air pressure and vacuum sources. The sample size used is 3 in. (7.5 cm) diameter x 3-1/8 in. (8 cm) long, but other sample sizes could be used. Typical measurements are presented to show repeatability and time required for permeability testing. The equipment has been used for permeabilities as low as 1 x 10-11 cm/sec. Concrete with lower permeability would require equipment modifications and/or longer measurement times.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer