Title: Crack Repair--An Engineer's Perspective

Author(s): Thomas S. Kline

Publication: Concrete International

Volume: 13

Issue: 6

Appears on pages(s): 47-49

Keywords: cracking (fracturing); evaluation; performance; repairs; quality assurance; quality control; site preparation; General

DOI:

Date: 6/1/1991

Abstract:
When untreated crack widths exceed ACI limits, repair programs are usually recommended by engineering professionals. This article reviews what those programs are and the proper procedures that should be followed.




  