Paper describes the modifications made to a previously developed CANMET test method to measure the permeability of concrete and discusses test results to determine the reproducibility of the test method. Briefly, the test method consists of measuring the uniaxial water flow through cylinders (125 mm high with a diameter of 150 mm) under a pressure of 3.5 MPa. A large number of concrete specimens with water-cement ratios of 0.65 and 0.80 were tested. A limited number of test specimens having w/c of 0.22 and 0.27 were also tested. Test results show that the within-batch variation for the test method is high, and this is probably due to the heterogenous nature of the concrete. For concrete with w/c of 0.22 and 0.27, there was no outflow of water, and this technique in the present form may not be suitable for measuring the permeability of very high strength concrete.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer