Title: Aramid Fabric as a Reinforcement for Concrete

Author(s): Janusz Kasperkjewicz and Hans W. Reinhardt

Publication: Symposium Paper

Volume: 138

Issue:

Appears on pages(s): 149-162

Keywords: beams (supports); bending; cracking (fracturing); ductility; fabric; fiber reinforced plastics; prestressing; reinforced concrete; Structural Research

DOI: 10.14359/3924

Date: 9/1/1993

Abstract:
Several researchers have used aramid fibers as prestressing tendons and as chopped fibers in concrete because of their high strength and chemical resistance. In this investigation, an aramid fabric is used as bending reinforcement in concrete beams. Cracking, bending capacity, and ductility are determined experimentally. It is shown how effective aramid fabric can be if applied in several layers as tensile reinforcement.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.