Title: Pavement Costs and Quality: A Consumer's Report

Author(s): Robert G. Packard

Publication: Concrete International

Volume: 16

Issue: 8

Appears on pages(s): 36-38

Keywords: asphalts; concrete; maintenance; pavements; Construction

DOI:

Date: 8/1/1994

Abstract:
This report compares the performance and costs of concrete and asphalt pavements. Included are the expected service life of new pavements as reported by several state and federal agencies and examples of pavement performance in several states. Initial pavement costs, maintenance costs, life-cycle costs, and rehabilitation costs are compared. The information is documented with 20 references.




  