Title: High-Performance Concrete: Stretching the Paradigm

Author(s): Stephen W. Forster

Publication: Concrete International

Volume: 16

Issue: 10

Appears on pages(s): 33-34

Keywords: creep properties; environments; heat transfer; loads (forces); high-performance concrete; pumped concrete; General

DOI:

Date: 10/1/1994

Abstract:
Over the last decade, the term "high-performance concrete" (HPC) has more and more come into popular use as an ideal we should all strive for. There seems to be universal agreement that production and use of HPC is a worthy goal; however, an additional systematic discussion of the concept may be in order to help clarify what it is we all are seeking. In the course of this discussion the author hopes to expand, or at least reposition, the paradigm or "box" each of us has constructed in our own minds to encompass, and often confine, HPC.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.