Title: 
            Behavior of Ultrasonic Pulses in Fresh Concrete
        
        
            Author(s): 
            S. Popovics, R. Silva-Rodrigez, J. S. Popovics, and V. Martucci
        
        
            
                Publication: 
                Symposium Paper
            
            
                Volume: 
                143
            
            
                Issue: 
                
            
            
                Appears on pages(s): 
                207-226
            
            
                Keywords: 
                cement pastes; compressive strength; construction; tests; fresh concretes; quality control; setting (hardening); ultrasonic tests;  velocity; Materials Research
            
            
                DOI: 
                10.14359/4318
            
        
        
            Date: 
            5/1/1994
        
        
            Abstract:
            Describes a laboratory investigation of an ultrasonic method that has the potential to become, through further research, a valuable tool for the nondestructive quality control of concrete during construction.  The primary objective of the work is to characterize the development of internal structure of the portland cement paste portion of concrete from very early ages on by making use of the behavior of propagated ultrasonic pulses. To do that, however, a suitable ultrasonic method first had to be developed, since quite a few publications reported difficulties with such measurements in fresh  pastes due to high attenuation.  Velocity and attenuation of longitudinal ultrasonic pulses were measured at regular intervals in fresh concretes. The first measurements were usually  performed 10 min after mixing and continued up to the age of 28 days. Three concretes of different compositions were tested. This paper concentrates on measurements at very early ages.  The instrumentation, test setup, and testing procedure are described. The velocity and attenuation results, as well as their interpretation, are then presented. For instance, it is shown that the time of initial set is close to a minimum on the pulse velocity-versus-age relationship, as well as a maximum on the attenuation-versus-age relationship.