Title: Polyester Concrete for Bridge DeckOverlays

Author(s): D. N. O'Connor and M. "Saiid" Saiidi

Publication: Concrete International

Volume: 15

Issue: 12

Appears on pages(s): 36-39

Keywords: bonding; chlorides; compressive strength; cracking (fracturing); deicing; resurfacing; spalling; temperature; Materials Research

DOI:

Date: 12/1/1993

Abstract:
The study presented in this paper was undertaken to determine the sensitivity of polyester concrete compressive strength to an increase in temperature; the effects of temperature cycling on compressive strength; the bonding strength of polyester concrete to portland cement concrete; and the modulus of elasticity of polyester concrete.




  