International Concrete Abstracts Portal

  


Title: Studies on Alkali-Carbonate Reaction

Author(s): Tang Mingshu, Deng Min, Lan Xianghui, and Han Sufen

Publication: Materials Journal

Volume: 91

Issue: 1

Appears on pages(s): 26-29

Keywords: alkali-carbonate reaction; carbonate aggregates; concretes; Materials Research

DOI: 10.14359/4446

Date: 1/1/1994

Abstract:
The main points with respect to alkali-carbonate reaction are described and discussed in detail. They include: 1) mechanism of expansion; 2) preventive measures; 3) cases of deterioration in China; 4) a rapid method to determine the reactivity of carbonate rock; and 5) comparison of alkali-silica reaction with alkali-carbonate reaction.