International Concrete Abstracts Portal

  


Title: Inspection and Repair of a Concrete Wharf

Author(s): M. Maage, S. Helland, J. E. Carlsen, and M. Ronne

Publication: Symposium Paper

Volume: 145

Issue:

Appears on pages(s): 797-810

Keywords: chlorides; concretes; corrosion; deterioration; inspection; latex; marine atmospheres; mortars (material); repairs; service life; silica fume; water content; wharves; Construction

DOI: 10.14359/4509

Date: 5/1/1994

Abstract:
Reinforcement corrosion due to chloride ingress is the most common cause of concrete deterioration in Norway. A wharf with dimensions of 270 x 25 m was built in 1965 to 1966 and required partial repairs in 1980, 1986, and 1989 to 1990. The repair work included some research and development. The conclusion of the 1989 inspection was that no corrosion activity was evident in the earlier repaired areas. Repair mortar with silica fume had somewhat lower chloride ingress and significantly higher electrical resistivity than mortar without silica fume. Latex addition to the repair mortar showed the same effect, as well as a reduced water content. The main conclusion is that materials and working procedures used for the 1980 repair have resulted in a satisfactory service life of at least 10 years.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer