Title: 325.1R-67: Design of Concrete Overlays for Pavements

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 5

Keywords: pavements

DOI:

Date: 1/1/1967

Abstract:

Note: 325.1R-67 is No Longer Available.

Presents information on bonded concrete resurfacing. Consideration is also given to concrete overlays on flexible pavements. Design procedures which will give dependable results are presented.