International Concrete Abstracts Portal

  


Title: Porosity and Permeability of Mortar Specimens Incorporating PEO113–b–PS218 Micelles

Author(s): D.A. Koleva, K. van Breugel, G. Ye, J. Zhou, G. Chamululu, and E.A.B. Koenders

Publication: Symposium Paper

Volume: 267

Issue:

Appears on pages(s): 101-110

Keywords: mortar; permeability; polymer nano-aggregates; porosity.

DOI: 10.14359/51663286

Date: 10/1/2009

Abstract:
This work presents results from an on-going investigation on the microstructural properties of cement-based materials in the presence of very low concentration of polymeric nano-aggregates. The hereby discussed properties are mainly porosity and permeability of mortar specimens, containing 0.5 g/L (0.03 lb/ft3 ) (mixing water) Poly(ethylene oxide)-block-Polystyrene (PEO113-b-PS218) stabilized micelles. The coefficient of water permeability, K, for the samples cast with nano-aggregates was found to be significantly lower, 3.65 e–14 m/s, compared to the control specimen, 3.7 e–8 m/s. Apparently, even a very low concentration of PEO113-b-PS218 micelles is able to significantly reduce water permeability at early ages. The phenomena are most likely denoted to re-distribution and transformation of hydration products in the matrix, the micelles contributing to restructuring of the pore space and altering the cement hydration mechanisms due to their specific amphiphilic properties.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.