High-Early-Strength Engineered Cementitious Composites for Fast, Durable Concrete Repair—Material Properties

International Concrete Abstracts Portal

  


Title: High-Early-Strength Engineered Cementitious Composites for Fast, Durable Concrete Repair—Material Properties

Author(s): Mo Li and Victor C. Li

Publication: Materials Journal

Volume: 108

Issue: 1

Appears on pages(s): 3-12

Keywords: compressive; concrete repair; cracking; ductility; durability; flexural; high-early-strength engineered cementitious composites; shrinkage; tensile

DOI: 10.14359/51664210

Date: 1/1/2011

Abstract:
The lack of durability in concrete structures worldwide demands fast and durable repairs. To address this need, high-early-strength engineered cementitious composites (HES-ECC) were recently developed for concrete repair applications in which minimum operations disruption is desired. A detailed characterization of HES-ECC’s compressive, tensile, flexural, and shrinkage properties at different ages is reported in this paper. HES-ECC achieves a compressive strength of 23.59 ± 1.40 MPa (3422.16 ± 203.33 psi) in 4 hours and 55.59 ± 2.17 MPa (8062.90 ± 315.03 psi) in 28 days. Under uniaxial tension, HES-ECC exhibits tensile strain-hardening behavior with a strain capacity greater than 2.5%. Its flexural strength exceeds twice that of concrete with similar compressive strength. Under restrained shrinkage conditions, HES-ECC forms microcracks with a self-controlled crack width below 50 μm (0.002 in.). The combination of these properties suggests that HES-ECC material is highly suitable for fast and durable concrete repairs with shortened downtime and improved longterm durability.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer