Title: Investigation of Efficient Anchorage Systems for Shear and Torsion Retrofitting of Box Girder Bridges

Author(s): R. Kalfat, R. Al-Mahaidi, and G. Williams

Publication: Symposium Paper

Volume: 275

Issue:

Appears on pages(s): 1-20

Keywords: CFRP, Concrete, Strengthening, Bond strength, Uni-directional, Bi-directional, Fabric, Anchorage

DOI: 10.14359/51682452

Date: 3/1/2011

Abstract:
Carbon Fibre reinforced Polymers (CFRP) have become an effective solution to upgrade and strengthen existing box girder bridges in flexure, shear and torsion. The introduction of CFRP strain limitations to prevent premature delamination together with the increasing strengthening demands and the necessity for use of fibres of increasing stiffness and thickness has resulted in a very poor CFRP material utilisation levels achieved in practice. An effective method to increase CFRP material utilisation is by appropriately anchoring the ends of the CFRP. In this paper, a study into CFRP end anchorage solutions is presented which formed the basis of the experimental program. Both uni-directional and bi-directional fabric was applied to the ends of CFRP laminates and tested under direct shear loading. Uni-directional fabric was oriented both horizontally across and parallel to the direction of the laminate. In all cases it was found that the anchorages solutions tested resulted in a distribution of fibre-to-adhesive bond stresses over a greater length, width of concrete and could potentially result full CFRP utilisation and laminate rupture.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer