Title: Durability and Performance of the Pervious Concrete Overlay at MNROAD

Author(s): John T. Kevern, Kejin Wang, and Vernon R. Schaefer

Publication: Symposium Paper

Volume: 282

Issue:

Appears on pages(s): 1-12

Keywords: Pervious concrete, Concrete overlay, Durability, Freeze-Thaw, Sustainability, Stormwater management

DOI: 10.14359/51683641

Date: 12/27/2011

Abstract:
This paper presents the results of studies conducted to develop a self-consolidating Portland Cement Pervious Concrete (PCPC) for overlay applications to reduce roadway noise, reduce splash and spray, and to improve friction as a surface wearing course. A variety of mixture variables were characterized for workability to develop a mixture for mechanized placement. During the fall of 2008, a 100 mm (4 in.) thick pervious concrete overlay on traditional concrete was constructed at a test facility. Construction is described as well as results of field tests to characterize the condition of the pavement seven months following construction. Performance testing of the overlay section included bond strength, permeability, skid resistance, and noise generation. The results of these studies show that effective PCPC overlays can be designed for wearing course applications.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer