Material Characterization of the Concrete-Epoxy Interface under FRP Uwraps

International Concrete Abstracts Portal

  


Title: Material Characterization of the Concrete-Epoxy Interface under FRP Uwraps

Author(s): Jaeha Lee and Maria M. Lopez

Publication: Symposium Paper

Volume: 286

Issue:

Appears on pages(s): 1-12

Keywords: Concrete, FRP, FRP Uwrap, Fracture mechanics, Interface

DOI: 10.14359/51683909

Date: 5/1/2012

Abstract:
This study focuses on the characterization of the fracture properties of the concrete-epoxy interface (CEI) under FRP sheets and FRP Uwraps. In particular, the Mode I and Mode II fracture energies are obtained with and without the effect of the FRP Uwrap anchor. Results indicate that fracture energy of the CEI increases due to the confining effect of Uwrap. These material properties, along with a proposed bond-slip model, are used in numerical simulations of concrete elements strengthened with externally bonded FRP sheets and anchored with FRP Uwraps. Results show that the characterization of the fracture properties of the CEI is needed to accurately predict the complex behavior of the CEI under the FRP Uwrap.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer