International Concrete Abstracts Portal

  


Title: Particle Arrangements in Freshly-Mixed Mortars: Basis for Modeling

Author(s): Sidney Diamond

Publication: JCI

Volume: 5

Issue: 3

Appears on pages(s): 277 - 283

Keywords:

DOI: 10.3151/jact.5.277

Date: 1/1/2007

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »  



  