Title: Evaluation Method of Tensile Behavior of Corroded Reinforcing Bars Considering Radius Loss

Author(s): Di Qiao, Hikaru Nakamura, Yoshihito Yamamoto, Taito Miura

Publication: JCI

Volume: 13

Issue: 3

Appears on pages(s): 135 - 146

Keywords:

DOI: 10.3151/jact.13.135

Date: 1/1/2015