Title: Investigation of Bacterial Activity on Compressive Strength of Cement Mortar in Different Curing Media

Author(s): Hemalatha Thiyagarajan, Srinivasan Maheswaran, Maitri Mapa, Sarayu Krishnamoorthy, Bhuvaneshwari Balasubramanian, Avadhanam Ramachandra Murthy, Nagesh R. Iyer

Publication: JCI

Volume: 14

Issue: 4

Appears on pages(s): 125 - 133

Keywords:

DOI: 10.3151/jact.14.125

Date: 1/1/2016