International Concrete Abstracts Portal

  


Title: Review of the Current State of Knowledge on the Effects of Radiation on Concrete

Author(s): Thomas M. Rosseel, Ippei Maruyama, Yann Le Pape, Osamu Kontani, Alain B. Giorla, Igor Remec, James J. Wall, Madhumita Sircar, Carmen Andrade, Manuel Ordonez

Publication: JCI

Volume: 14

Issue: 7

Appears on pages(s): 368 - 383

Keywords:

DOI: 10.3151/jact.14.368

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.