Title: Examination of Strength Model for the Cementitious Material Containing Aluminous Cement

Author(s): Hirokatsu Mori, Takayasu Itoh, Toshiyuki Takahashi, Takashi Akatsu, Etsuo Sakai

Publication: JCI

Volume: 14

Issue: 9

Appears on pages(s): 607 - 613

Keywords:

DOI: 10.3151/jact.14.607

Date: 1/1/2016

Abstract: