Title: Railway bridge over river Ebre in Zaragoza

Author(s): Medina Mediana, C.

Publication: ACHE

Volume: 56

Issue: 238

Appears on pages(s): 27 - 33

Keywords:

DOI:

Date: 1/8/2005

Abstract:
The new bridge over river Ebre in Zaragoza constituted a part of the duplication of the railway infrastructure that joints the cities of Zaragoza and Huesca. The bridge is 305 metres long with the following span distribution 40 + 50 + 125 + 50 + 40 metres. This structure has been designed with the current high speed criteria giving special attention to the design of the details that assure a correct maintenance and the durability of the structure. The central span has been solved with a metallic arch with rigid lower deck.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.