Title: Bridge over the river Ebro at Riba-Roja

Author(s): de Villar Luengo, J.M.; Simón-Talero Muñoz, J.M.;

Publication: ACHE

Volume: 51

Issue: 216

Appears on pages(s): 17 - 25

Keywords:

DOI:

Date: 1/3/2000

Abstract:
The bridge over the river Ebro at Riba-Roja is a prestressed concrete continuous bridge build by the cantilever construction method. The girder is 10.6 m width, being three spans 100 + 150 + 100 m length supported by V shape piers. Some considerations concerning fundamentals and design of the bridge and a slight description of the main typological and geometrical characteristics of the bridge are presented. Description of some of incidences during construction and solutions defined for correcting them are also included in this article. The bridge was open for users in 1997.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.