International Concrete Abstracts Portal

  


Title: Post-tensioning in building

Author(s): Llombart Jaques, J. A.

Publication: ACHE

Volume: 51

Issue: 215

Appears on pages(s): 127 - 139

Keywords:

DOI:

Date: 1/1/2000

Abstract:
The article describes the basic characteristics of post-tensioned slabs and compares them with conventional reinforced concrete solutions. The post-tensioning technique with unbonded tendons has not beeen very common in Spain until now, and has been used only rarely. Some of the most representative buildings constructed in Spain are mentioned and, by way of reference, some of the buildings constructed in other countries in the past few year are described


ACI International Partner, ACHE Spain, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.