Title: Time dependent presstress losses. Experimental results

Author(s): Romo Martín, J.; Corres Peiretti, H.

Publication: ACHE

Volume: 41

Issue: 177

Appears on pages(s): 121 - 124

Keywords:

DOI:

Date: 1/8/1990

Abstract:
Experimental results concerning time dependent losses in prestressed concrete elements is presented. These results have been provided through a theoretical and experimental research programme which is being carried out at the ETSICCP of the UPM.