Title: Damage detection of prestressed concrete beams by the method of curvature of the elastic

Author(s): Germán D. Ercolani, Néstor F. Ortega, Daniel H. Felix

Publication: ACHE

Volume: 69

Issue: 284

Appears on pages(s): 39 - 48

Keywords: Pre-stressed concrete, Damage detection, Cracks, Finite elements, Elasticity

DOI:

Date: 1/1/2018

Abstract:
At the time of inspecting and ensuring the safety of an existing structure, it is important to have proper techniques to detect the presence of damage in that structure. In this work, a study is made of the method of curvature of the elasticity, applied specifically to the detection of bending cracks in pre-stressed concrete beams, a typology widely used in highway bridges. The studies were performed on a set of three-dimensional models, using the finite element method. Different sensitivity analyses were carried out to determine, successfully, the required parameters for the implementation of the method of curvature of the elasticity in practice.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer