Title: Steel fiber reinforced concrete, engineering and practise

Author(s): Lucea Martínez, I.

Publication: ACHE

Volume: 35

Issue: 152

Appears on pages(s): 129 -

Keywords:

DOI:

Date: 1/5/1984

Abstract:


ACI International Partner, ACHE Spain, International Partner Access