Title:
2-D Debonding Evolution in FRP Strengthened Plates Under Combined Loading
Author(s):
Shai Feldfogel; and Oded Rabinovitch
Publication:
Web Session
Volume:
Issue:
Appears on pages(s):
Keywords:
DOI:
Date:
10/14/2017
Abstract:
This international symposium attracts interest from researchers, practitioners, and manufacturers involved in the use of fiber-reinforced polymers (FRPs) as reinforcement for concrete structures. This includes the use of FRP reinforcement in new construction and FRP for strengthening and rehabilitation of existing structures.