Title: 
            Experimental Study of Interior Glass Fiber-Reinforced Polymer-Reinforced Concrete Slab-Column Connections under Lateral Cyclic Load
        
        
            Author(s): 
            Mohamed Eladawy, Mohamed Hassan, and Brahim Benmokrane
        
        
            
                Publication: 
                Structural Journal
            
            
                Volume: 
                116
            
            
                Issue: 
                6
            
            
                Appears on pages(s): 
                165-180
            
            
                Keywords: 
                cyclic loading; design codes; dissipated energy; drift capacity; ductility; glass fiber-reinforced polymer bars; punching shear; reinforced concrete slab-column connection
            
            
                DOI: 
                10.14359/51716803
            
        
        
            Date: 
            11/1/2019
        
        
            Abstract:
            The feasibility of using fiber-reinforced polymers (FRPs) as internal reinforcement for a totally reinforced concrete (RC) structure immune to corrosion essentially pertains to strength, stiffness, and deformation capacity in resisting seismic loads has become questionable. Nevertheless, no experiments have yet been conducted on the punching-shear behavior of FRP-reinforced concrete (FRPRC) slab-column connections subjected to lateral reversal cyclic
loading. Consequently, current FRP-RC design guidelines and codes in North America contain no seismic provisions. This has been the main impetus to conduct the first-ever experimental study on the punching shear behavior of glass-FRP (GFRP) slab-column connections under the combination of gravity and lateral reversed cyclic loading. Four full-scale interior slab-column connections were constructed and tested to investigate the influence of flexural-
reinforcement type (GFRP and steel bars), reinforcement ratio, and gravity load intensity on the punching shear performance. All test specimens were identical and measured 2500 x 2500 mm with a thickness of 200 mm. A column measuring 300 x 300 mm extended 700 mm at its center above and below the slab surfaces. The results revealed that the GFRP-RC specimens possessed adequate strength and deformation capacity against punching-shear failure during and after reserved lateral cyclic-load conditions. The GFRP-RC specimens achieved lateral interstory drift capacities over 1.50% satisfying the limits in CSA A23.3 and ACI 421.3R. The GFRP-RC specimens also had adequate drift-ductility indexes, dissipated energy, and connection stiffness. Moreover, the GFRP bar strains at the ultimate lateral-drift ratio were less than the guaranteed tensile strength by 42%. No rupture of the GFRP bars and bond failure or slip were observed during the test.
        
     
    
    
    
            Related References:
                
                        Ali, M., and El-Salakawy, E., 2016, “Seismic Performance of GFRP-Reinforced Concrete Rectangular Columns,” Journal of Composites for Construction, ASCE, V. 20, No. 3, p. 04015074. doi: 10.1061/(ASCE)CC.1943-5614.0000637
                    
                        ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.
                    
                         ACI Committee 440, 2004, “Guide Test Methods for Fiber-Reinforced Polymers (FRPs) for Reinforcing or Strengthening Concrete Structures (ACI 440.3R-04),” American Concrete Institute, Farmington Hills, MI, 40 pp.
                    
                         ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI.
                    
                        ASTM D7205M, 2011, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 12 pp.
                    
                        Canadian Standards Association, 2012, “Design and Construction of Building Structures with Fiber Reinforced Polymers (CAN/CSA S806-12),” CSA Group, Rexdale, ON, Canada, 198 pp.
                    
                        Canadian Standards Association, 2014a, “Canadian Highway Bridge Design Code (CAN/CSA S6-14),” CSA Group, Rexdale, ON, Canada, 798 pp.
                    
                        Canadian Standards Association (CSA), 2014b, “Design of Concrete Structures for Buildings,” (CSA-A23.3 M-14), CSA Group, Rexdale, ON, Canada, 240 pp.
                    
                        Canadian Standards Association (CSA), 2015, “Specification for Fiber-Reinforced Polymers (CAN/CSA S807-15),” CSA Group, Rexdale, ON, Canada, 27 pp.
                    
                        Drakatos, I. S.; Muttoni, A.; and Beyer, K., 2016, “Internal Slab-Column Connections under Monotonic and Cyclic Imposed Rotations,” Engineering Structures, V. 123-501-516, Sept.
                    
                        Dulude, C.; Hassan, M.; Ahmed, E. A.; and Benmokrane, B., 2013, “Punching Shear Behaviour of Two-Way Flat Concrete Slabs Reinforced with GFRP Bars,” ACI Structural Journal, V. 110, No. 5, Sept.-Oct. pp. 723-734.
                    
                        Elshamandy, M. G.; Farghaly, A. S.; and Benmokrane, B., 2018, “Experimental Behavior of GFRP-Reinforced Concrete Columns under Lateral Cyclic Load,” ACI Structural Journal, V. 115, No. 2, Mar., pp. 337-349.
                    
                        Emam, M.; Marzouk, H.; and Hilal, S., 1997, “Seismic Response of Slab-Column Connections Constructed with High-Strength Concrete,” ACI Structural Journal, V. 94, No. 2, Mar.-Apr., pp. 94-S19.
                    
                        Ghomi, S. K., and El-Salakawy, E., 2015, “Seismic Behavior of Beam-Column Joints Reinforced with GFRP Bars and Stirrups,” Journal of Composites for Construction, ASCE, V. 15, No. 6, p. 04015019. doi: 10.1061/(ASCE) CC.1943-5614.0000220
                    
                        Gouda, A., and El-Salakawy, E., 2015, “Punching Shear Strength of GFRP-RC Interior Slab-Column Connections Subjected to Moment Transfer,” Journal of Composites for Construction, ASCE, doi: 10.1061/(ASCE) CC.1943-5614.0000597.10.1061/(ASCE)
                    
                        Hassan, M.; Ahmed, E. A.; and Benmokrane, B., 2013, “Punching-Shear Strength of GFRP-Reinforced Concrete Flat Slabs,” Canadian Journal of Civil Engineering, V. 40, No. 10, Apr., pp. 951-960. doi: 10.1139/cjce-2012-0177
                    
                        Hussein, A., and El-Salakawy, E., 2018, “Punching Shear Behavior of Glass Fiber-Reinforced Polymer-Reinforced Concrete Slab-Column Interior Connections” ACI Structural Journal, V. 115, No. 4, July, pp. 1075-1088. doi: 10.14359/51702134.
                    
                        Joint ACI-ASCE Committee 421, 2010, “Guide to Seismic Design of Punching Shear Reinforcement in Flat Plates (ACI 421.2R-10),” American Concrete Institute, Farmington Hills, MI.
                    
                        Lee, J. H.; Yoon, Y. S.; and Mitchell, D., 2009, “Improving Punching Shear Behavior of Glass Fiber-Reinforced Polymer Reinforced Slabs,” ACI Structural Journal, V. 106, No. 4, July-Aug., pp. 427-434.
                    
                        Mady, M.; El-Ragaby, A.; and El-Salakawy, E., 2011, “Seismic Behavior of Beam-Column Joints Reinforced with GFRP Bars and Stirrups,” Journal of Composites for Construction, ASCE, V. 15, No. 6, pp. 875-886. doi: 10.1061/(ASCE)CC.1943-5614.0000220
                    
                        Marzouk, H.; Osman, M.; and Hussein, A., 2001, “Cyclic Loading of High-Strength Lightweight Concrete Slabs” ACI Structural Journal, V. 98, No. 2, Mar.-Apr., pp. 90-101.
                    
                        Matthys, S., and Taerwe, L., 2000, “Concrete Slabs Reinforced with FRP Grids. I: One-Way Bending,” Journal of Composites for Constructions, ASCE, V. 4, No. 3, pp. 145-153. doi: 10.1061/(ASCE)1090-0268(2000)4:3(145)
                    
                        Megally, S., 1998, “Punching Shear Resistance of Concrete Slabs to Gravity and Earthquake Forces,” PhD thesis, Department of Civil Engineering, Calgary University, Calgary, AB, Canada, 504 pp.
                    
                        Megally, S., and Ghali, A., 1994, “Design Considerations for Slab-Column Connections in Seismic Zones,” ACI Structural Journal, V. 91, No. 3, May-June, pp. 303-314.
                    
                        Megally, S., and Ghali, A., 2000, “Seismic Behavior of Edge Column-Slab Connections with Stud Shear Reinforcement,” ACI Structural Journal, V. 97, No. 1, Jan.-Feb., pp. 53-60.
                    
                        National Research Council of Canada, 2015, “National Building Code of Canada,” NBCC 2015, Ottawa, ON, Canada, 1222 pp.
                    
                        Osman, M.; Marzouk, H.; and Helmy, S., 2000, “Behavior of High-Strength Lightweight Concrete Slabs under Punching Loads,” ACI Structural Journal, V. 97, No. 3, May-June, pp. 99-097.
                    
                        Ospina, C. E.; Alexander, S. D. B.; and Roger Cheng, J. J., 2003, “Punching of Two-Way Concrete Slabs with Fiber-Reinforced Polymer Reinforcing Bars or Grids,” ACI Structural Journal, V. 100, No. 5, Sept.-Oct., pp. 589-598.
                    
                        Pan, A., and Moehle, J. P., 1989, “Lateral Displacement Ductility of Reinforced Concrete Flat Plates,” ACI Structural Journal, V. 86, No. 3, May-June, pp. 250-258.
                    
                        Park, R., 1989, “Evaluation of Ductility of Structures and Structural Assemblages from Laboratory Testing,” Bulletin of the New Zealand National Society for Earthquake Engineering, V. 22, No. 3, pp. 155-166.
                    
                        Robertson, I., and Johnson, G., 2006, “Cyclic Lateral Loading of Non-ductile Slab-Column Connections,” ACI Structural Journal, V. 103, No. 3, May-June, pp. 356-364.
                    
                        Robertson, N. I., and Durrani, A. J., 1992, “Gravity Load Effect on Seismic Behavior of Interior Slab-Column Connection,” ACI Structural Journal, V. 89, No. 1, Jan.-Feb., pp. 37-45.
                    
                        Zaghloul, A., 2007, “Punching Shear Strength of Interior and Edge Column-Slab Connections in CFRP Reinforced Flat Plate Structures Transferring Shear and Moment,” PhD thesis, Department of Civil and Environmental Engineering, Carleton University, Ottawa, ON, Canada, 372 pp.