Proposed Slenderness Limit for Glass Fiber-Reinforced Polymer-Reinforced Concrete Columns Based on Experiments and Buckling Analysis

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Slenderness Limit for Glass Fiber-Reinforced Polymer-Reinforced Concrete Columns Based on Experiments and Buckling Analysis

Author(s): Waseem Abdelazim, Hamdy M. Mohamed, Mohammad Z. Afifi, and Brahim Benmokrane

Publication: Structural Journal

Volume: 117

Issue: 1

Appears on pages(s): 241-254

Keywords: columns; design codes; first and second-order analysis; GFRP reinforcing bars; instability and buckling; lateral displacement; reinforced concrete; short and slender columns; slenderness ratio; stiffness

DOI: 10.14359/51718073

Date: 1/1/2020

Abstract:
To develop design provisions for concrete columns reinforced with fiber-reinforced polymer (FRP) bar for North American codes and guidelines (ACI 440.1R, CSA S806), a slenderness limit below which it is acceptable to ignore the induced second-order effects must be determined. Nevertheless, limited attempts have been made to define a safe slenderness limit for such columns. Therefore, this study aimed at experimentally and analytically investigating the buckling behavior of 12 full-scale concrete columns reinforced with glass FRP (GFRP) with slenderness ratios of 14, 17, 23, 26, and 33 under concentric loading. The impact of longitudinal reinforcement ratios and confining levels on the performance of slender GFRP-reinforced concrete (GFRP-RC) columns is also presented. Test results indicate that the GFRP reinforcement contributed significantly to resisting the applied compression loads and resulted in failure modes similar to that of the counterpart steel-reinforced concrete columns at different slenderness ratios. In addition, a theoretical buckling analysis considering a total of 50 test specimens, assembled from the current study and the literature, was developed to verify the applicability of Euler-Johnson’s stability envelope as well as the reduced and incremental modulus theories to FRP-RC columns. Good correlation was observed between the experimental results and the models developed analytically. Based on the experimental data and the developed buckling analysis, the safe limit of the slenderness ratio for FRP-RC columns bent in single curvature of 18 is proposed.

Related References:

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with FRP Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 88 pp.

Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., 2014, “Axial Capacity of Circular Concrete Columns Reinforced with GFRP Bars and Spirals,” Journal of Composites for Construction, ASCE, V. 18, No. 1, Feb., p. 04013017. doi: 10.1061/(ASCE)CC.1943-5614.0000438

ASTM D2584-08, 2008, “Standard Test Method for Ignition Loss of Cured Reinforced Resins,” ASTM International, West Conshohocken, PA, 3 pp.

ASTM C39/C39M-17b, 2017, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 8 pp.

Bažant, Z. P.; Cedolin, L.; and Tabbara, M. R., 1991, “New Method of Analysis for Slender Columns,” ACI Structural Journal, V. 88, No. 4, July-Aug., pp. 391-401.

Canadian Standards Association (CSA), 2012, “Design and Construction of Building Components with Fiber Reinforced Polymers (CAN/CSAS806-12),” CSA Group, Mississauga, ON, Canada, 198 pp.

Canadian Standards Association (CSA), 2014, “Design of Concrete Structures (CSA A23.3-14),” CSA Group, Rexdale, ON, Canada, 298 pp.

De Luca, A.; Matta, F.; and Nanni, A., 2010, “Behavior of Full-Scale Glass Fiber-Reinforced Polymer Reinforced Concrete Columns under Axial Load,” ACI Structural Journal, V. 107, No. 5, Sept.-Oct., pp. 589-596.

Engesser, F., 1889, “Uber die Knickfestigkeit gerader Stabe,” Zeitschrift fur Architektur und lngenieurwesen, V. 35 (Section 8.1).

Guérin, M.; Mohamed, H. M.; Benmokrane, B.; Shield, C. K.; and Nanni, A., 2018, “Effect of Glass Fiber-Reinforced Polymer Reinforcement Ratio on Axial-Flexural Strength of Reinforced Concrete Columns,” ACI Structural Journal, V. 115, No. 4, July, pp. 1049-1061. doi: 10.14359/51701279

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017a, “Axial Load-Moment Interaction Diagram of Circular Concrete Columns Reinforced with CFRP Bars and Spirals: Experimental and Theoretical Investigations,” Journal of Composites for Construction, ASCE, V. 21, No. 2, Jan., p. 04016092. doi: 10.1061/(ASCE)CC.1943-5614.0000748

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017b, “Experimental Study of Circular High-Strength Concrete Columns Reinforced with GFRP Bars and Spirals under Concentric and Eccentric Loading,” Journal of Composites for Construction, ASCE, V. 21, No. 2, Jan., p. 04016078. doi: 10.1061/(ASCE)CC.1943-5614.0000734

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017d, “Strength of Circular HSC Columns Reinforced Internally with Carbon-Fiber-Reinforced Polymer Bars under Axial and Eccentric Loads,” Construction and Building Materials, V. 141, pp. 366-378. doi: 10.1016/j.conbuildmat.2017.02.117

Hadhood, A.; Mohamed, H. M.; Benmokrane, B.; Nanni, A.; and Shield, C. K., 2019, “Assessment of Design Guidelines of Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 116, No. 4, July, pp. 193-207. doi: 10.14359/51715663

Hadhood, A.; Mohamed, H. M.; Ghrib, F.; and Benmokrane, B., 2017c, “Efficiency of Glass-Fiber Reinforced-Polymer (GFRP) Discrete Hoops and Bars in Concrete Columns under Combined Axial and Flexural Loads,” Composites. Part B, Engineering, V. 114, No. 6, pp. 223-236. doi: 10.1016/j.compositesb.2017.01.063

Hadi, M. N.; Karim, H.; and Sheikh, M. N., 2016, “Experimental Investigations on Circular Concrete Columns Reinforced with GFRP Bars and Helices under Different Loading Conditions,” Journal of Composites for Construction, ASCE, V. 20, No. 4, p. 04016009. doi: 10.1061/(ASCE)CC.1943-5614.0000670

Hales, T. A.; Pantelides, C. P.; and Reaveley, L. D., 2016, “Experimental Evaluation of Slender High-Strength Concrete Columns with GFRP and Hybrid Reinforcement,” Journal of Composites for Construction, ASCE, V. 20, No. 6, Dec., p. 04016050 doi: 10.1061/(ASCE)CC.1943-5614.0000709

MacGregor, J. G.; Breen, J. E.; and Pfrang, E. O., 1970, “Design of Slender Concrete Columns,” ACI Journal Proceedings, V. 67, No. 1, Jan., pp. 6-28.

Maranan, G. B.; Manalo, A. C.; Benmokrane, B.; Karunasena, W.; and Mendis, P., 2016, “Behavior of Concentrically Loaded Geopolymer-Concrete Circular Columns Reinforced Longitudinally and Transversely with GFRP Bars,” Engineering Structures, V. 117, No. 15, June, pp. 422-436. doi: 10.1016/j.engstruct.2016.03.036

Mirmiran, A.; Shahawy, M.; and Beitleman, T., 2001b, “Slenderness Limit for Hybrid FRP Concrete Columns,” Journal of Composites for Construction, ASCE, V. 5, No. 1, Feb., pp. 26-34. doi: 10.1061/(ASCE)1090-0268(2001)5:1(26)

Mirmiran, A.; Yuan, W.; and Chen, X., 2001a, “Design for Slenderness in Concrete Columns Internally Reinforced with Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 98, No. 1, Jan.-Feb., pp. 116-125.

Mohamed, H. M.; Abdel-Baky, H.; and Masmoudi, R., 2010, “Nonlinear Stability Analysis of Concrete Filled Fiber-Reinforced Polymer-Tube Columns: Experimental and Theoretical Investigation,” ACI Structural Journal, V. 107, No. 6, Nov.-Dec., pp. 699-708.

Mohamed, H. M.; Afifi, M. Z.; and Benmokrane, B., 2014, “Performance Evaluation of Concrete Columns Reinforced Longitudinally with FRP Bars and Confined with FRP Hoops and Spirals under Axial Load,” Journal of Bridge Engineering, ASCE, V. 19, No. 7, June, p. 04014020. doi: 10.1061/(ASCE)BE.1943-5592.0000590

Pantelides, C. P.; Gibbons, M. E.; and Reaveley, L. D., 2013, “Axial Load Behavior of Concrete Columns Confined with GFRP Spirals,” Journal of Composites for Construction, ASCE, V. 17, No. 3, June, pp. 305-313. doi: 10.1061/(ASCE)CC.1943-5614.0000357

Popovics, S., 1973, “A Numerical Approach to the Complete Stress-Strain Curve of Concrete,” Cement and Concrete Research, V. 3, No. 5, Sep., pp. 583-599. doi: 10.1016/0008-8846(73)90096-3

Shanley, F. R., 1947, “Inelastic Column Theory,” Journal of the Aeronautical Sciences, V. 14, No. 5, May, pp. 261-268. doi: 10.2514/8.1346

Sheikh, S. A., and Kharal, Z., 2018, “Replacement of Steel with GFRP for Sustainable Reinforced Concrete,” Construction and Building Materials, V. 160, pp. 767-774. doi: 10.1016/j.conbuildmat.2017.12.141

Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., 2012, “Concrete Columns Reinforced Longitudinally and Transversally with GFRP Bars,” ACI Structural Journal, V. 109, No. 4, July-Aug., pp. 551-558.

Xue, W.; Peng, F.; and Fang, Z., 2018, “Behavior and Design of Slender Rectangular Concrete Columns Longitudinally Reinforced with Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 115, No. 2, Mar., pp. 311-322. doi: 10.14359/51701131

Youssef, J., and Hadi, M. N., 2017, “Axial Load-Bending Moment Diagrams of GFRP Reinforced Columns and GFRP Encased Square Columns,” Construction and Building Materials, V. 135, pp. 550-564. doi: 10.1016/j.conbuildmat.2016.12.125

Zadeh, H. J., and Nanni, A., 2013, “Design of RC Columns Using Glass FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 17, No. 3, pp. 294-304. doi: 10.1061/(ASCE)CC.1943-5614.0000354

Zadeh, H. J., and Nanni, A., 2017, “Flexural Stiffness and Second-Order Effects in Fiber-Reinforced Polymer-Reinforced Concrete Frames,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr., pp. 533-544. doi: 10.14359/51689257


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer