Isothermal Strength Development Models of Ultra-High- Performance Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Isothermal Strength Development Models of Ultra-High- Performance Concrete

Author(s): Thomas E. Allard, Matthew W. Priddy, Isaac L. Howard, and Jay Shannon

Publication: Materials Journal

Volume: 117

Issue: 1

Appears on pages(s): 175-185

Keywords: isothermal curing; strength development; ultra-high-performance concrete

DOI: 10.14359/51719075

Date: 1/1/2020

Abstract:
Ultra-high-performance concrete (UHPC) has progressively gained interest because of its favorable strength and durability properties. Considering applications of heat treatment and mass concrete, understanding the direct relationship between curing temperature and time is informative for construction decisions (such as formwork type and time of removal) to maximize performance per unit cost of UHPCs, as they can differ from conventional concrete. Limited datasets are currently available to ascertain the degree of change related to UHPC mechanical properties as a function of curing temperature and conditions. This study presents a systematic experimental program to investigate the effect of isothermal and submerged conditions on the rate and extent of compressive strength and elastic modulus development for UHPC, followed by development of numerical models that capture these effects with reasonable accuracy. Although the final elastic modulus appears to be unaffected by temperature, much higher compressive strength was achieved with higher curing temperatures compared to ambient conditions, and both properties were successfully modeled.

Related References:

1. Shah, S. P., and Konsta-Gdoutos, M. S., “Uncoupling Modulus of Elasticity and Strength,” Concrete International, V. 39, No. 11, 2017, pp. 37-42.

2. ACI Committee 363, “Report on High-Strength Concrete (ACI 363R-13),” American Concrete Institute, Farmington Hills, MI, 2013.

3. Williams, E.; Graham, S.; Reed, P.; and Rushing, T., “Laboratory Characterization of Cor-Tuf Concrete with and without Steel Fibers,” ERDC/GSL TR-09-22.

4. Green, B. H.; Moser, R. D.; Scott, D. A.; and Long, W. R., “Ultra-High-Performance Concrete History and Usage by the Corps of Engineers,” Advances in Civil Engineering Materials, V. 4, No. 2, 2015, pp. 132-143.

5. Graybeal, B., “Material Property Characterization of Ultra-High-Performance Concrete,” Report FHWA-HRT-06-103 McLean, VA, Aug. 2006.

6. ACI Committee 239, “Ultra-High-Performance Concrete: An Emerging Technology Report (ACI 239R-18),” American Concrete Institute, Farmington Hills, MI, 2018.

7. Liu, Z.; Chen, W.; Zhang, W.; Zhang, Y.; and Lv, H., “Complete Stress-Strain Behavior of Ecological Ultra-High-Performance Composite under Uniaxial Compression,” ACI Materials Journal, V. 114, No. 5, Sept.-Oct. 2017, pp. 783-794. doi: 10.14359/51689899

8. Gajda, J., Mass Concrete for Buildings and Bridges, Portland Cement Association, EB547 Skokie, IL, 2007.

9. Graybeal, B., Ultra-High-Performance Concrete, Technical Note FHWA-HRT-11-083 McLean, VA, 2011.

10. Ahmad, S.; Hakeem, I.; and Azad, A. K., “Effect of Curing, Fibre Content and Exposures on Compressive Strength and Elasticity of UHPC,” Advances in Cement Research, V. 27, No. 4, 2015, pp. 233-239. doi: 10.1680/adcr.13.00090

11. Alsalman, A.; Dang, C. N.; Prinz, G. S.; and Hale, W. M., “Evaluation of Modulus of Elasticity of Ultra-High-Performance Concrete,” Construction and Building Materials, V. 153, 2017, pp. 918-928. doi: 10.1016/j.conbuildmat.2017.07.158

12. Habel, K.; Viviani, M.; Denarié, E.; and Brühwiler, E., “Development of the Mechanical Properties of an Ultra-High-Performance Fiber Reinforced Concrete (UHPFRC),” Cement and Concrete Research, V. 36, No. 7, 2006, pp. 1362-1370. doi: 10.1016/j.cemconres.2006.03.009

13. Wan, L.; Wendner, R.; Liang, B.; and Cusatis, G., “Analysis of the Behavior of Ultra High-Performance Concrete at Early Age,” Cement and Concrete Composites, V. 74, 2016, pp. 120-135. doi: 10.1016/j.cemconcomp.2016.08.005

14. Berry, M.; Snidarich, R.; and Wood, C., “Development of Non-Proprietary Ultra-High-Performance Concrete,” Report FHWA/MT-17-010/8237-001 Bozeman, MT, Dec. 2017.

15. Howard, I. L.; Carey, A.; Burcham, M.; Scott, D. A.; Shannon, J. D.; Moser, R. D.; and Horstemeyer, M. F., Mechanical Behavior of Cor-Tuf Ultra-High-Performance Concrete Considering Aggregate and Paste Effects. Report ERDC/GSL TR-18-31, U.S. Army Corps of Engineers Engineer Research and Development Center, Vicksburg, MS, 2018, pp. 74.

16. Prem, P. R.; Murthy, A. R.; and Bharatkumar, B. H., “Influence of Curing Regime and Steel Fibres on the Mechanical Properties of UHPC,” Magazine of Concrete Research, V. 67, No. 18, 2015, pp. 988-1002. doi: 10.1680/macr.14.00333

17. Maage, M., “Strength and Heat Development in Concrete: Influence of Fly Ash and Condensed Silica Fume,” Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete—Proceedings of the Second International Conference, Madrid, Spain, SP-91,V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1986, pp. 923-940.

18. Korpa, A., and Trettin, R., “Very High Early Strength of Ultra-High-Performance Concrete Containing Nanoscale Pozzolans Using the Microwave Heat Curing Method,” Advances in Cement Research, V. 20, No. 4, 2008, pp. 175-184. doi: 10.1680/adcr.2008.20.4.175

19. Sbia, L. A.; Peyvandi, A.; Harsini, I.; Lu, J.; Abideen, S. U.; Weerasiri, R. R.; Balachandra, A. M.; and Soroushian, P., “Study on Field Thermal Curing of Ultra-High-Performance Concrete Employing Heat of Hydration,” ACI Materials Journal, V. 114, No. 5, Sept.-Oct. 2017, pp. 733-744. doi: 10.14359/51689677

20. Carino, N. J., “The Maturity Method: Theory and Application,” Cement, Concrete, and Aggregates V. 6, No. 2, Winter 1984, pp. 61-73.

21. Carino, N. J., and Lew, H. S., “The Maturity Method: From Theory to Application,” Proceedings of the 2001 Structures Congress & Exposition, American Society of Civil Engineers, Reston, VA, May 2001.

22. Cervera, M.; Faria, R.; Oliver, J.; and Prato, T., “Numerical Modelling of Concrete Curing, Regarding Hydration and Temperature Phenomena,” Computers & Structures, V. 80, No. 18-19, 2002, pp. 1511-1521. doi: 10.1016/S0045-7949(02)00104-9

23. Kim, J.-K.; Moon, Y.-H.; and Eo, S.-H., “Compressive Strength Development of Concrete with Different Curing Time and Temperature,” Cement and Concrete Research, V. 28, No. 12, 1998, pp. 1761-1773. doi: 10.1016/S0008-8846(98)00164-1

24. Lee, C.; Lee, S.; and Nguyen, N., “Modeling of Compressive Strength Development of High-Early-Strength-Concrete at Different Curing Temperatures,” International Journal of Concrete Structures and Materials, V. 10, No. 2, 2016, pp. 205-219. doi: 10.1007/s40069-016-0147-6

25. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11),” American Concrete Institute, Farmington Hills, MI, 2011, 473 pp.

26. Logan, S. R., “The Origin and Status of the Arrhenius Equation,” Journal of Chemical Education, V. 59, No. 4, 1982, pp. 279-281. doi: 10.1021/ed059p279

27. Kim, J. K.; Han, S. H.; and Lee, K. M., “Estimation of Compressive Strength by a New Apparent Activation Energy Function,” Cement and Concrete Research, V. 31, No. 2, 2001, pp. 217-225. doi: 10.1016/S0008-8846(00)00481-6

28. ACI Committee 209, “Prediction of Creep, Shrinkage, and Temperature Effects in Concrete Structures (ACI 209R-13),” American Concrete Institute, Farmington Hills, MI, 2013.

29. D’Aloia, L., and Chanvillard, G., “Determining the ‘Apparent’ Activation Energy of Concrete Ea – Numerical Simulations of the Heat of Hydration of Cement,” Cement and Concrete Research, V. 32, No. 8, 2002, pp. 1277-1289. doi: 10.1016/S0008-8846(02)00791-3

30. Cervera, M.; Oliver, J.; and Prato, T., “Thermo-Chemo-Mechanical Model for Concrete. I: Hydration and Aging,” Journal of Engineering Mechanics, ASCE, V. 125, No. 9, 1999, pp. 1018-1027. doi: 10.1061/(ASCE)0733-9399(1999)125:9(1018)

31. Faria, R.; Azenha, M.; and Figueiras, J. A., “Modelling of Concrete at Early Ages: Application to an Externally Restrained Slab,” Cement and Concrete Composites, V. 28, No. 6, 2006, pp. 572-585. doi: 10.1016/j.cemconcomp.2006.02.012

32. Ulm, F., and Coussy, O., “Modeling of Thermochemomechanical Couplings of Concrete at Early Ages,” Journal of Engineering Mechanics, ASCE, V. 121, No. 7, 1995, pp. 785-794. doi: 10.1061/(ASCE)0733-9399(1995)121:7(785)

33. Di Luzio, G., and Cusatis, G., “Hygro-Thermo-Chemical Modeling of High-Performance Concrete. I: Theory,” Cement and Concrete Composites, V. 31, No. 5, 2009, pp. 301-308. doi: 10.1016/j.cemconcomp.2009.02.015

34. Fairbairn, E. M. R.; Silvoso, M. M.; Toledo Filho, R. D.; Alves, J. L. D.; and Ebecken, N. F. F., “Optimization of Mass Concrete Construction Using Genetic Algorithms,” Computers & Structures, V. 82, No. 2-3, 2004, pp. 281-299. doi: 10.1016/j.compstruc.2003.08.008

35. Howard, I. L.; Shannon, J.; Cost, V. T.; and Stovall, M., “Davis Wade Stadium Expansion and Renovation: Performance of Concrete Produced with Portland-Limestone Cement, Fly Ash, and Slag Cement,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 12, 2015. doi: 10.1061/(ASCE)MT.1943-5533.0001305

36. Rossum, G. V., “Python Tutorial,” Technical Report CS-R9526, Centrum voor Wiskunde en Informatica (CWI), Amsterdam, May 1995.

37. Oliphant, T. E., “Python for Scientific Computing,” Computing in Science & Engineering, V. 9, No. 3, 2007, pp. 10-20. doi: 10.1109/MCSE.2007.58


ALSO AVAILABLE IN:

Electronic Materials Journal



  

Edit Module Settings to define Page Content Reviewer