Title: RAP-12 Concrete Repair by Shotcrete Application

Author(s): ACI Committee E706

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 6

Keywords:

DOI:

Date: 4/13/2011

Abstract:
FIELD GUIDE TO CONCRETE REPAIR APPLICATION PROCEDURES Concrete Repair by Shotcrete Application The shotcrete process is typically used to restore structural integrity, increase concrete cover over reinforcement, or both. It’s typically used when forming requirements are difficult or prohibitively expensive or as another repair tool in the designer’s and contractor’s tool kits.




  