Ductile Concrete End-Diaphragms of Slab-on-Girder Concrete Bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ductile Concrete End-Diaphragms of Slab-on-Girder Concrete Bridges

Author(s): Esteban Villalobos-Vega and Guillermo Santana

Publication: Structural Journal

Volume: 119

Issue: 1

Appears on pages(s): 119-130

Keywords: accelerated bridge construction (ABC) solutions; bridge; ductility; end-diaphragm beam; experimental test; hybrid system; precast concrete; seismic resistance

DOI: 10.14359/51733140

Date: 1/1/2022

Abstract:
In this paper, the results of the proposed ductile precast concrete end-diaphragm beams for the transverse seismic resistance and protection of the substructure of slab-on-girder concrete bridges, tested at the facilities of LanammeUCR structural laboratory, University of Costa Rica, are detailed and discussed. The proposal can be used as part of an accelerated bridge construction (ABC) solution for moderate- to high-risk seismic areas. The hysteretic results showed adequate energy dissipation performance of the transverse end-diaphragm beams system; however, the envelopes obtained in both load directions evidenced a marked difference: the negative envelope showed a more noticeable ductile behavior and close enough to the predicted theoretical monotonic curve than the positive envelope. The damage observed at the precast concrete diaphragm beams was negligible, and the concrete deterioration was concentrated in the corners of the connections with the bridge girders, where the grout mortar at the joint gap evidenced a poor performance. Even if the bridge girders showed cracking both due to shear and flexure, the residual crack width was low: on average 0.10 mm. The final conclusion is that even if the test showed some issues that have to be revised, the system has the potential to demonstrate an outstanding performance under lateral seismic load.

Related References:

1. Yen, W. P.; Chen, G.; Buckle, I.; Allen, T.; Alzamora, D.; Ger, J.; and Arias, J. G., “Post-Earthquake Reconnaissance Report on Transportation Infrastructure: Impact of the February 27, 2010, Offshore Maule Earthquake in Chile,” Publication No. FHWA-HRT-11-030, Federal Highway Administration, McLean, VA, October 2011, 198 pp.

2. Zahrai, S. M., and Bruneau, M., “Ductile End-Diaphragms for Seismic Retrofit of Slab-on-Girder Steel Bridge,” Journal of Structural Engineering, ASCE, V. 125, No. 1, 1999, pp. 71-80. doi: 10.1061/(ASCE)0733-9445(1999)125:1(71)

3. Zahrai, S. M., and Bruneau, M., “Cyclic Testing of Ductile End Diaphragms for Slab-on-Girder Steel Bridges,” Journal of Structural Engineering, ASCE, V. 125, No. 9, 1999, pp. 987-996. doi: 10.1061/(ASCE)0733-9445(1999)125:9(987)

4. AASHTO, “Guide Specifications for LRFD Seismic Bridge Design,” second edition, American Association of State Highway and Transportation Officials, Washington, DC, 2011.

5. Stone, W. C.; Cheok, G. S.; and Stanton, J. F., “Performance of Hybrid Moment-Resisting Precast Beam-Colum Concrete Connections Subjected to Cyclic Loading,” ACI Structural Journal, V. 91, No. 2, Mar.-Apr. 1995, pp. 229-249.

6. Priestley, M. J. N.; Sritharan, S. S.; Conley, J. R.; and Stefano Pampanin, S., “Preliminary Results and Conclusions from the PRESSS Five-Story Precast Concrete Test Building,” PCI Journal, V. 44, No. 6, 1999, pp. 42-67. doi: 10.15554/pcij.11011999.42.67

7. Kim, J; Stanton, J.; MacRae, G.; Day, S.; and Sugata, M., “Cyclic Load Testing of Precast Hybrid Frame Connections,” Proceedings of the 13th World Conference on Earthquake Engineering, Vancouver, BC, Canada, August 1-6, 2004, Paper No. 1671, 15 pp.

8. Kurama, Y. C.; Sritharan, S.; Fleischman, R. B.; Restrepo, J. I.; Henry, R. S.; Cleland, N. M.; Ghosh, S. K.; and Bonelli, P., “Seismic-Resistant Precast Concrete Structures: State of the Art,” Journal of Structural Engineering, ASCE, V. 144, No. 4, 2018. doi: 10.1061/(ASCE)ST.1943-541X.0001972

9. Garlock, M. M.; Ricles, J. M.; and Sause, R., “Cyclic Load Test and Analysis of Bolted Top-and-Seat Angle Connections,” Journal of Structural Engineering, ASCE, V. 129, No. 12, 2003, pp. 1615-1625. doi: 10.1061/(ASCE)0733-9445(2003)129:12(1615)

10. Kurama, Y. C.; Weldon, B. D.; and Shen, Q., “Experimental Evaluation of Posttensioned Hybrid Coupled Wall Subassemblages,” Journal of Structural Engineering, ASCE, V. 132, No. 7, 2006, pp. 1017-1029. doi: 10.1061/(ASCE)0733-9445(2006)132:7(1017)

11. Weldon, B. D., and Kurama, Y. C., “Experimental Evaluation of Post-tensioned Precast Concrete Coupling Beams,” Journal of Structural Engineering, ASCE, V. 136, No. 9, 2010, pp. 1066-1077. doi: 10.1061/(ASCE)ST.1943-541X.0000212

12. Villalobos-Vega, E., and Santana-Barboza, L. G., “Experimental Study on Ductile Precast End-Diaphragms of Slab-on-Girder Concrete Bridges: Pre-test Analytical Study,” Proceedings of the 2016 PCI Convention and National Bridge Conference, Precast/Prestressed Concrete Institute, Nashville, TN, March 3-6, 2016, 18 pp.

13. Restrepo, J. I., and Rahman, A., “Seismic Performance of Self-Centering Structural Walls Incorporating Energy Dissipators,” Journal of Structural Engineering, ASCE, V. 133, No. 11, 2007, pp. 1560-1568. doi: 10.1061/(ASCE)0733-9445(2007)133:11(1560)

14. ASTM C31/C31M-15, “Standard Practice for Making and Curing Concrete Test Specimens in the Field,” ASTM International, West Conshohocken, PA, 2015, 6 pp.

15. ASTM C39/C39M-15a, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

16. ASTM C109/C109M-13e1, “Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50-mm] Cube Specimens),” ASTM International, West Conshohocken, PA, 2013, 10 pp.

17. ASTM C1611/C1611M-14, “Standard Test Method for Slump Flow of Self-Consolidating Concrete,” ASTM International, West Conshohocken, PA, 2014, 6 pp.

18. ASTM A416/A416M-15, “Standard Specification for Low-Relaxation, Seven-Wire Steel Strand for Prestressed Concrete,” ASTM International, West Conshohocken, PA, 2015, 4 pp.

19. ASTM A706/A706M-15, “Standard Specification for Deformed and Plain Low-Alloy Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

20. ASTM A709/A709M-15, “Standard Specification for Structural Steel for Bridges,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

21. ACI Innovation Task Group 5, “Acceptance Criteria for Special Unbonded Post-Tensioned Precast Structural Walls Based on Validation Testing and Commentary (ACI ITG-5.1-07),” American Concrete Institute, Farmington Hills, MI, 2008, 19 pp.

22. Park, R., “Evaluation of Ductility of Structures and Structural Assemblages from Laboratory Testing,” Bulletin of the New Zealand National Society for Earthquake Engineering, V. 22, No. 3, 1989, pp. 155-166. doi: 10.5459/bnzsee.22.3.155-166

23. Celik, O., and Sritharan, S., “An Evaluation of Seismic Design Guidelines Proposed for Precast Concrete Hybrid Frame Systems,” ISU-ERI-Ames Report ERI-04425, Precast/Prestressed Concrete-Manufacturers Association of California - University of Iowa, January 2004, 216 pp.

24. ACI Committee 224, Reapproved 2008, “Control of Cracking in Concrete Structures (ACI 224R-01),” American Concrete Institute, Farmington Hills, MI, 2001, 46 pp.

25. Hose, Y. D., and Seible, F., “Performance Evaluation Database for Concrete Bridge Components and Systems under Simulated Seismic Loads,” Report No. PEER 1999/11, Pacific Earthquake Engineering Research Center, University of California, Berkeley, Berkeley, CA, November 1999, 112 pp.

26. Alfawakhiri, F., and Bruneau, M., “Local Versus Global Ductility Demands in Simple Bridges,” Journal of Structural Engineering, ASCE, V. 127, No. 5, 2001, pp. 554-560. doi: 10.1061/(ASCE)0733-9445(2001)127:5(554)

27. Pampanin, S., “Living a New Era in Earthquake Engineering: Targeting Damage-Resisting Solutions to Meet Societal Expectations,” Proceedings of the Australian Earthquake Engineering Society 2012 Conference, Tweed Heads, Australia, Dec. 7-9, 2012, 23 pp.

28. White, S., and Palermo, A., “Controlled Damage Precast Connections for Accelerated Bridge Construction in Regions of High Seismicity,” Proceedings of the 2014 NZSEE Conference, Auckland, New Zealand, Mar. 21-23, 2014, 9 pp


ALSO AVAILABLE IN:

Electronic Structural Journal