Title: Prediction of Shear Strength of One-Way Slabs Voided by Circular Paper Tubes using Artificial Intelligence

Author(s): Iman Mansouri, Chang-Hwan Lee, and Paul O. Awoyera

Publication: Symposium Paper

Volume: 350

Issue:

Appears on pages(s): 132-141

Keywords: voided slab, one-way slab, shear strength, artificial neural network

DOI: 10.14359/51734319

Date: 11/1/2021

Abstract:
TUBEDECK, a one-way spanning voided composite slab, has been utilized in the construction field over the years to enhance the efficiency, constructability, and environmental performance of structures. TUBEDECK incorporates both cast-in-situ reinforced concrete slabs and profiled steel decks. However, there is a need to clarify the shear resistance capacity in this slab because the shear strength of the member reduces as concrete volume is eliminated to optimize flexural strength. Therefore, this study applied the artificial neural network (ANN) technique to determine the shear strength of TUBEDECK. By varying factors in the ANN features, several ANN models were developed. Out of many models developed, an optimal model was selected, having a maximum/mean relative errors of 5.1% in a dataset.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer