International Concrete Abstracts Portal

  


Title: ASCC Position Statement #45

Author(s):

Publication: Concrete International

Volume: 44

Issue: 6

Appears on pages(s): 54-55

Keywords: contract, contractor, cost, owner

DOI:

Date: 6/1/2022

Abstract:
Unpredictable and unstable market factors are beyond the control of the concrete contractor and make it difficult to maintain the costs and schedules reasonably anticipated at bid time. Early dialogue regarding pricing levels, mill orders, availability of price lock mechanisms, and delivery date projections can maximize benefits to the owner and help minimize project risk.




  