Title: Pozzolanic Reactivity of Supplementary Cementitious Materials

Author(s): Keshav Bharadwaj, O. Burkan Isgor, and W. Jason Weiss

Publication: Materials Journal

Volume: 120

Issue: 4

Appears on pages(s): 63-76

Keywords: pozzolanic reactivity test (PRT); reactivity; supplementary cementitious materials (SCMs); thermodynamic modeling

DOI: 10.14359/51738817

Date: 7/1/2023

Abstract:
As the number of potential supplementary cementitious materials (SCMs) increase, there is a need to determine their reactivity. Most recent methods to assess pozzolanic reactivity are based on measuring certain outputs such as heat release (Q), calcium hydroxide (CH) consumption, and nonevaporable water. This paper uses thermodynamic modeling to aid in the interpretation of these tests and the quantification of reactivity. It is shown that pozzolanic reactivity should be interpreted based on the SCM type. The presence of sulfates and carbonates during reactivity quantification alter the reaction of the Al2O3 phases, making the interpretation of the reactivity test results challenging. The reactivity of commercial SCMs should be interpreted specific to the type of SCM as described by ASTM International/AASHTO. A proposed interpretation for commercial SCMs is provided in this paper.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer